Battery · Case study
A label that stopped peeling in transit
Electrolyte splash was lifting a client’s existing labels before the batteries reached the dealer.
What changed
Zero field rejections across 1.2M units
01 / How it went
What actually happened.
Problem
Batteries were arriving at dealers with the main label lifted at one corner and the terminal label bleeding. The dealer was refusing them on sight, so a label worth a few paise was writing off a battery.
What we did
We ran the existing stock and ours side by side in full-strength electrolyte at bonnet temperature for a day, and showed the client both trays. The job moved onto our own battery paper, and the terminal label was redrawn a few millimetres clear of the post.
Result
Twelve months and 1.2 million units later, no field rejection has come back to the label. The client moved the rest of their range across the following quarter.
Got a problem
like this?
Tell us what is going wrong with the one you have now. That is usually the fastest way in.